The Investigation On The Function Of Floaters Using Glass Furnace Models

The results of model investigations concerning the influence of hydrodynamic barriers (floater) on the current patterns in the glass furnace as well as on the influence of the place and the depth of location of floaters are presented.

Author
A. Karkosa
Origin
Unknown
Journal Title
Szklo Ceram., 1971, 22, (6), 168-172