An Introduction To Materials For Glass Moulds

With key factors such as production costs and speed in mind, this article presents us with some information regarding the materials used to manufacture moulds for hollow glass production. Applications, morphology and characteristics are also looked into with comparisons given of thermal fatigue properties of gray, compacted ductile irons

Author
A Tiziani And Etal
Origin
Italy
Journal Title
Glass Machinery Plants & Accessories July/Aug 2006 62 - 66