The Interrelationship Between The Structures Of Borate Glasses And Crystals

A summary is presented of structural data for the crystalline polymorphs existing in a wide range of binary borate glass-forming systems and is used as a basis to propose a set of topolgical criteria for the formation of vitreous borate networks. It is shown that this yields considerable insight concerning the structural criteria for the formation of such networks, but that the information which can be obtained is limited by the fact that many of the relevant crystalline structures have not been determined.

Author
A C Wright Et Al
Origin
Reading University, Uk
Journal Title
Proc 2Nd Int Conference Borate Glasses, Crystals & Melts 1996 80-87
Sector
Special Glass
Class
S 3645

Request article (free for British Glass members)

The Interrelationship Between The Structures Of Borate Glasses And Crystals
Proc 2Nd Int Conference Borate Glasses, Crystals & Melts 1996 80-87
S 3645
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.