Interpretation Of Hydrated States Of Sodium Silicate Glasses By Infrared And Raman Analysis

Infrared spectra of thin films of hydrated sodium silicate glasses after heating at temperatures from 100 to 400 degrees C were measured in the spectral region from 400 to 4300 cm-1. Raman spectra of hydrated glasses were measured in the region from 100 to 1400 cm-1.