Interpretation Of The 57Fe Mossbauer Spectra Of Some Phosphate Glasses

This paper describes the application of a quadrupole splitting distribution fitting programme to various iron phosphate glasses.

Author
J S Brooks Et Al
Origin
Sheffield City Polytechnic
Journal Title
Physics & Chem Of Glasses 33 5 October 1992 167-170