Internal Pressure Strength Of Carbonated Beverage Bottles

Cetie Fact Sheet FS 04 has recently been updated. The data sheet gives guidance on the relationship between the internal pressure strength standards used for process control at the point of manufacture and the pressure strength standards applicable at the point of receipt of the bottles by the bottler and in the case of refillable bottles, the pressure strength standards which might be applicable to the pool of refillable bottles.