Internal Pressure Resistance Of Glass Containers (In Italian)

The bursting pressure strength of glass containers as a function of shape and weight can be predicted by a statistical approach or by a theoretical calculation using finite element theory. The advantages and limitations of these methods are discussed with particular reference to manufacturing defects such as thickness variations and out-of-round shapes.

Author
T Toninato Et Al
Origin
Unknown
Journal Title
Rivista Della Stazione Del Vetro 13 2 1983 63-69