Interim Study Of A Chrome-Free, High-Efficiency Checker Setting In A Container Glass Furnace

Reinstallation in another furnace of bricks that had been in service for 30 months operation is reported. The bricks gave satisfactory performance for a further 13 months in the new location.

Author
W J Kivala, H E Wolfe
Origin
Unknown
Journal Title
Ceramic Engng Sci Proc 1988 9 3-4 315-328