Interfacial Reactions Between A Lead Borosilicate Glass Dielectric Coating And An Al/Sic Metal Matrix Composite

A PbO rich borosilicate glass has been developed as a thick film, dielectric coating for an Al/SiC particle reinforced metal matrix composite (MMC). Sessile drop experiments were performed to investigate interfacial reactions. The wetting behaviour of the glass, highly fluid at the bonding temperature (500-600 deg C), was found to be a function of atmosphere, temperature and time. Coatings applied under air exhibited ~10% porosity attributed to the production of CO2 gas through the oxidation of SiC at the glass/MMC interface. This may occur via oxygen diffusion through the glass drop from the air to the interface or via a redox reaction between the SiC and the lead oxide component of the glass at the glass/MMC interface, the latter generating free lead metal as a waste product.

Author
S J Ison Et Al
Origin
University Of Warwick, Uk
Journal Title
Phys Chem Glasses 41 5 2000 267-271
Sector
Special Glass
Class
S 2057

Request article (free for British Glass members)

Interfacial Reactions Between A Lead Borosilicate Glass Dielectric Coating And An Al/Sic Metal Matrix Composite
Phys Chem Glasses 41 5 2000 267-271
S 2057