Interfacial Energy In Phase-Separated Glasses From Emulsion Rheology

Classical theories of emulsion rheology yield information on the deformation of a liquid drop dispersed into another liquid matrix phase. By connecting the deformational and relaxation, respectively, and the capillary number of the dispersed phase, interfacial energy can be estimated. This was applied to demixing borosilicate and lead borate glasses, which are known to exhibit significant form anisotropy after elongation. Interfacial energies in these two systems were calculated based on graphical data or prior isothermal elongation experiments. the method is discussed in terms of experimental difficulties.s It might provide an alternative way to overcome the obvious lack of information on interfacial energies in glasses.

Author
L Wondraczek Et Al
Origin
University Claushthal, Germany
Journal Title
Jacs 88 6 2005 1673-1675
Sector
Special Glass
Class
S 2968

Request article (free for British Glass members)

Interfacial Energy In Phase-Separated Glasses From Emulsion Rheology
Jacs 88 6 2005 1673-1675
S 2968
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.