Interfacial Characterisation Of Silicon Carbide Fibre/Lihia-Alumina-Silica Glass Matrix Composites

The development of the carbon-rich inerphase in Nicalon SiC fibre/Li2O-Al2O3-SiO2 glass matrix composites was examined as a function of processing parameters with the use of high-resolution scanning electron microscopy and Auger electron spectroscopy.

Author
J Homeny, J R Vanvalzah, M A Kelly
Origin
University Of Illinois
Journal Title
J Am Ceram Soc 1990 73 7 2954-2059