Interactions Between Ruthenia-Based Resistors And Cordierite-Glass Substrates In Low-Temperature Co-Fired Ceramics

Low-temperature co-fired ceramics (LTCCs) that are composed of a Ru02-based resistor and a cordierite-glass substrate have been sintered at temperatures of 850 deg C and 900 deg C. The microstructure of the resistor/substrate interface has been investigated using scanning and transmission electron microscopy and its correlation to the overall resistance has been discussed.

Author
C Ting Et Al
Origin
Nat Sun Yat-Sen University, Taiwan
Journal Title
J Am Ceram Soc 83 12 2000 2945-2953
Sector
Glass Ceramics
Class
GC 403

Request article (free for British Glass members)

Interactions Between Ruthenia-Based Resistors And Cordierite-Glass Substrates In Low-Temperature Co-Fired Ceramics
J Am Ceram Soc 83 12 2000 2945-2953
GC 403
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.