Interactions Between Bioactive Glasa Nd Collage: A Review And New Perspectives

This review brings together for the first time the sequence of studies that have been done in both in-vitro and in vivo environments that have led to the basic science understanding of collagen-bioactive glass interactions. These studies and this understanding are the basis for the long-term clinical success of medical devices and osteogenic stimulating powders of bioactive glass and the ability of the bioactive glass powders to repair and protect teeth when used in oral care products.

Author
L L Hench & D Greenspan
Origin
Imperial College London & Spinode Consulting, Florida, Usa
Journal Title
J Aust Ceram Soc 49 2 2013 1-40
Sector
Special Glass
Class
S 4020

Request article (free for British Glass members)

Interactions Between Bioactive Glasa Nd Collage: A Review And New Perspectives
J Aust Ceram Soc 49 2 2013 1-40
S 4020
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.