Interaction Of Microstructure Development With Viscous Flow Processes Ing Glass

Measurements in glasses undergoing phase separation showed a large increase of viscosity with heat-treatment time. A correlation of this effect with electron micrographs of the structure indicated that the change in velocity was related to an increase in the size of the microstructure. A theoretical analysis is presented which is based on a model relating point-to=point variations in molecular environments to viscous flow processes in glass.

Author
J.H. Simmons Et Al
Origin
Unknown
Journal Title
Journal Of Non-Crystalline Solids 1974 14 302-309
Sector
Primary Papers
Class
PP 610

Request article (free for British Glass members)

Interaction Of Microstructure Development With Viscous Flow Processes Ing Glass
Journal Of Non-Crystalline Solids 1974 14 302-309
PP 610
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.