Interaction Of Glass Surfaces With Environment And Strength Variation Using Weibull Analysis

In this work, the effects on the strength of typical industrial glasses (pyrex and soda-lime-silica rods), after extended exposure at a constant temperature, in acidic, neutral and alkaline environments, are investigated. SEM is used for the examination of the surfaces of samples, with the intention of explicating the interaction of the surfaces with environment. In addition, mechanical three-point bending tests are performed for the glass rods, in order to calculate their strength, followed by Weibull analysis, in an attempt to analyse the strength variation of glasses, for all conditions tested.

Author
N P Avdelidis Et Al
Origin
Unknown
Journal Title
Riv Staz Sper Vetro 30 6 2000 117-120
Sector
Special Glass
Class
S 2182

Request article (free for British Glass members)

Interaction Of Glass Surfaces With Environment And Strength Variation Using Weibull Analysis
Riv Staz Sper Vetro 30 6 2000 117-120
S 2182
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.