Intelligent Cooking Systems

One of the most innovative products of recent decades recently celebrated a significant anniversary and at the same time notched up another record: It is 25 years since the first "Ceran" glass-ceramic cooktop by Schott appeared on the market. And the 35 millionth cooktop has just come off the production line in Mainz.