An Integrated Scheme For Rapid Analysis Of Glass And Other Silicate Materials Without Using Costly Platinum Wares And The Toxic Kcn

The analysis of various samples of soda-lime glasses is described, the results showing satisfactory conformity with those obtained by standard methods.