Integrated Photoelasticity For Residual Stress Measurement

Integrated photoelasticity facilitates calculation of residual stresses on the surfaces of hollow glassware, as well as stress distribution through the wall.

Author
H Aben & K Sharples
Origin
Estonian Academy Of Sci & Sharples Stress Eng Ltd
Journal Title
Glass Prod Tech Int 1994 203-204
Sector
Container glass
Class
C 658