Inspection Systems For Cosmetic And Perfume Bottles

Stolzle Flaconnage manufactures high quality glass containers for the cosmetics and perfumery market, supplying to companies such as Christian Dior, Yves Saint Laurent, Estee Lauder and Revlon. As part of its £9.3m investment in high quality, state-of-the-art technology, Stolzle has purchased two inspection systems, one on-line and one off-line.