Inspection Equipment In The Glass Container Industry: Future Direction And Recent Developments

Fillers continue to ask for both package differentiation and light-weight containers. This article identifies some trends in the industry, the impact these trends have on inspection and quality control equipment, how this equipment will contribute to the industry's success, and the author's opinion on future inspection strategy.