Inorganic Colloidal Glasses - Relations Between Preparation And Structure

Sodium silicate solutions were dried to form water containing amorphous solids. "Synthetic" sols were also prepared by dispensing silica colloids in NaOH solution. The size of the colloids was varied by using different grades of pyrogenic silica as precursors. The resulting sodium silicate liquids were dried at temperatures between 40-120 deg C under controlled climatic conditions. The residual water contents were determined gravimetrically. A gradual solidification of the solutions during drying is observed. Under appropriate drying conditions, amorphous materials are obtained. The process of solidification is interpreted as immobilisation of the colloids due to the extraction of water, thus reducing the distances between the colloidal particles. A correlation between structural parameters and drying conditions is discussed.

Author
H Roggendorf Et Al
Origin
Martin Luther University, Germany
Journal Title
9Th Int Conf Corning - Phys Chem Glasses 46 4 2005 439-443
Sector
Special Glass
Class
S 3070

Request article (free for British Glass members)

Inorganic Colloidal Glasses - Relations Between Preparation And Structure
9Th Int Conf Corning - Phys Chem Glasses 46 4 2005 439-443
S 3070
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.