An Innovative Point Fixing Device For Architectural Glazing, From Concept To Application

The safety performance of structural laminated glass panels is generally nullified if the link to the rear load-bearing structure is not able to retain the panels after glass breakage. To overcome this difficulty, an innovative point-fixing system that exploits the mechanical properties of ionoplast polymer interlayers has been developed. Performance test confirm that laminated glass connected with the new device exhibits a noteworthy resistance and interesting post-glass-breakage performances.

Author
G Royer-Carfagni & M Silvestri
Origin
Dept Civil Engineering, University Of Parma, Italy
Journal Title
Glass-Tech Int 4/09 84-88
Sector
Flat glass
Class
F 2834

Request article (free for British Glass members)

An Innovative Point Fixing Device For Architectural Glazing, From Concept To Application
Glass-Tech Int 4/09 84-88
F 2834
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.