Innovative 64Mm Quad Gob Forming System Installed

USA-based Quantum Engineered Products has successfully installed and commissioned an innovative 64mm quad gob forming system on a production line within a manufacturing plant in southern Germany. The plant specialises in the production of high quality pharmaceutical glass containers. In the initial stages of the project, the Quantum equipment was tested and evaluated on a portion of an existing IS machine. The results proved positive, therefore, the German plant made the decision to completely outfit a recently purchased IS machine with the Quantum forming system. For more information please visit: www.quantumforning.com

Author
Un-named
Origin
Unknown
Journal Title
www.Quantumforming.com
Sector
Container glass
Class
C 5780

Request article (free for British Glass members)

Innovative 64Mm Quad Gob Forming System Installed
www.Quantumforming.com
C 5780
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.