Innovations In Architectural Laminated Glass

2001's annual worldwide DuPont Benedictus Awards, which has now reached its 9th edition, received entries ranging from the addition to a Japanese imperial temple to the design of modern telephone booths. Special recognition was given to project areas such as residential, functional and space-saving. Student participants were asked to concentrate on architectural problems regarding the use of laminated glass in a theoretical design issue and, at the same time, investigating the many applications and uses of such glass as a building material.

Author
Un-named
Origin
Unknown
Journal Title
Glass-Tech Int 6/2001 109-118
Sector
Flat glass
Class
F 1295

Request article (free for British Glass members)

Innovations In Architectural Laminated Glass
Glass-Tech Int 6/2001 109-118
F 1295
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.