Innovation In Glass Fusion

This article analyses, in the light of current requirements, the technological innovations developed in the last twenty years in the field of glass fusion. In particular, it examines the latest technological advances with regard to firing, electrical furnaces, rapid refining, anti NOx systems, and cullet treatment.

Author
J L Barton
Origin
Unknown
Journal Title
Vetro Informazione 77 September-October 1993
Sector
Refractories
Class
R 116

Request article (free for British Glass members)

Innovation In Glass Fusion
Vetro Informazione 77 September-October 1993
R 116