Ink Jet Technology Provides Decorating Flexiblity

Decorating glassware using ink jet technology provides a cost effective alternative to conventional decorating methods. In this artricle, Dawn Hudock provides an overview of current technology and outlines the possibilities for use.

Author
D Hudock
Origin
Videojet Systems Int Inc, Usa
Journal Title
Glass 75 7 1998 212
Sector
Domestic glass
Class
D 348