Initial Dissolution Rate Of The International Simple Glass As A Function Of Ph And Temperature Measured Using Microchannel Flow-Through Test Method

International Simple Glass (ISG) is a six-component alumino-borosilicate glass developed as a reference benchmark glass for six nations collaborating study on high-level nuclear waste glass dissolution/corrosion mechanism. In this study, aqueous dissolution tests were performed for the ISG using micro-channel flow-through (MCFT) method to evaluate the initial dissolution rate of glass matrix, ro, precisely and systematically as a function of solution pH and temperature. The test results indicated that the ro shows a "V-shaped" pH dependence with a bottom at around pH4 at each temperature. Compared with Japanese reference glass of PO 798, for which the ro showed a !U-shaped" pH dependence with a bottom at around pH6 in a previous study - the ISG shows the higher dissolution rate at basic pH and lower dissolution rate at neutral to acidic pH. The results also indicated that the ro increases with temperature according to an Arrhenius law, and the apparent activation energy evaluated from Arrhenius relation is 62-77 [kJ/mol] at any pH from 3-10, which suggests the initial dissolution of ISG proceeds controlled by a surface-reaction mechanism in this pH range.

Author
Y Inagaki Et Al
Origin
Kyushu University, Fukuoka, Japan
Journal Title
Int J Appl Glass Sci 4 4 2013 317-327
Sector
Special Glass
Class
S 4070

Request article (free for British Glass members)

Initial Dissolution Rate Of The International Simple Glass As A Function Of Ph And Temperature Measured Using Microchannel Flow-Through Test Method
Int J Appl Glass Sci 4 4 2013 317-327
S 4070