Inhomogeneity And Mesostructure Of Oxide Coating On Glass

Inhomogeneity (in depth) of Ti,Al, and ZR oxide coatings deposited on glass using a sol-gel method is attributed both to the effect of the meostructure of oxide components and to quantum transfer of wavelength light. Substancial deviation from the additivity of the refractive index is observed for TiO2 - ZrO2 coatings. Homogeneity in depth and RI additivity can be attained if one of the components is present in excess.

Author
N A Sergeev Etal
Origin
Tomsk Polytechnical University, Russia
Journal Title
Glass And Ceramics 57 5-6 2000 205 - 207