An Ingenious Combination Of Creativity And Engineering

Machinery manufacturer Tamglass Engineering Oy, has completely redisigned and re-engineered its automotive glass factory in Tampere, Finalnd. The plant has an important additional role as an R & D facility where new machinery designs are tested in production conditions.