Infrared Thermography In The Production Of Glass Lamps

This paper describes the practical application of infrared thermography and concludes by discussing the most essential features of a thermal imaging system for implementing the technique successfully.

Author
Bo Wallin
Origin
Agema Infrared Systems Ltd
Journal Title
Glass Prod Tech Int 1995 176-179
Sector
Domestic glass
Class
D 213