Infrared Technology At The Hot End

In this article the authors argue that the use of hot end infrared inspection and process control systems is more effective than cold end monitoring.

Author
P Schreuders & P Van Tilburg
Origin
Xpar Vision, Netherlands
Journal Title
Glass Worldwide May-June/09 60-61