Infrared Spectroscopic Analysis Of Water Incorporated In The Structure Of Industrial Soda-Lime-Silica Glasses

This paper illustrates a method for the determination of the water content of glasses by infrared transmittance spectroscopy from the extinctions of the bands due to free and hydrogen-bonded hydroxyl groups dissolved in the glass. The procedure is discussed in detail, highlighting the sources of random and systematic errors and what can be done to improve the interlaboratory reproducibility.

Author
F Beotti-Bianchini & L De Riu
Origin
Stazione Sperimentale Del Vetro, Italy
Journal Title
Glastech Ber Glass Sci Technol 68 7 1995 228-240
Sector
Special Glass
Class
S 900

Request article (free for British Glass members)

Infrared Spectroscopic Analysis Of Water Incorporated In The Structure Of Industrial Soda-Lime-Silica Glasses
Glastech Ber Glass Sci Technol 68 7 1995 228-240
S 900
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.