Infrared Radiation Thermometers In The Glass Industry

An account is given of the use of infrared thermometers for temperatures of regenerator packings, crowns, bridge walls, port arches, tank roofs and forehearths. Aspects of the installation and maintenance of permanently installed thermometers are also considered.