Influences Of Zirconia And Silicon Nucleating Agents On The Devitrification Of Lio2.Al2O3.6Sio2 Glasses

The effects of Zi and ZrO2 dopants on the crystallisation and phase transformation process in lithia aluminosilicate glasses were investigated using differential thermal analysis, X-ray powder diffractometry and high-resolution transmission electron microscopy interactively.

Author
J-Y Hsu, R F Speyer
Origin
The New York State College Of Ceramics At Alfred University
Journal Title
J Am Ceram Soc 1990 73 12 3585-3593