The Influence Of Water Present In The Batch On The Fining Process Of Lead Crystal Containing More Than 24% Percent By Weight Of Pbo

The paper deals with the effect of chemically and physically bound water in the batch on the fining process of lead crystal containing more than 24 wt% of PbO. The influence of water contained in the batch that effects eventually the water content in the glass melt was investigated under laboratory conditions from the viewpoint of its effects on the total degree of fining, the surface tension and glass viscosity. The role of K2O- containing raw materials characterised by different contents in chemically bonded water as well as the effect of various water content used for physical batch wetting on above mentioned parameters are discussed by taking into account the production economy and the protection of the environment at the same time.

Author
M. Rada And J Vrovsky
Origin
Vscht Praha Technicka, Praha, Czech Republic
Journal Title
Advanced Materials Research Vols 39-40 (2008) 489-492
Sector
Special Glass
Class
S 3422

Request article (free for British Glass members)

The Influence Of Water Present In The Batch On The Fining Process Of Lead Crystal Containing More Than 24% Percent By Weight Of Pbo
Advanced Materials Research Vols 39-40 (2008) 489-492
S 3422
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.