The Influence Of Upon The Structural Chemical And Physical Properties Of Phosphate Glasses.

Structural studies have been carried out to provide information on the role of the fluorine ion when introduced into phosphate glasses.

Author
J.J. Videau Et Al.
Origin
Unknown
Journal Title
Glass Technology 1983 24 (3) 171
Sector
Primary Papers
Class
PP 868

Request article (free for British Glass members)

The Influence Of Upon The Structural Chemical And Physical Properties Of Phosphate Glasses.
Glass Technology 1983 24 (3) 171
PP 868