The Influence Of Technological Parameters On The Properties Of Foam Glass (Polish)

Laboratory tests on the development of foam glass ceramics are described. The temperature and times used were for preheating 650C and 60 minutes, for foaming 1160C and 75 minutes and for crystallisation 860C and 15 minutes.