Influence Of Tank Geometry And The Electrode Arrangement On The Flow And Temperature Distribution At Different Loads In A Glass Tank Furnace

Using a physical model to a scale of 1:15, the flow distrubition and isotherm patterns were determined for a hollow ware tank with a melting area of 68m2 at different loads, both with and without electric boosting. In addition, the tank geometry was varied.

Author
H. Pieper And J. Rosenthal.
Origin
Unknown
Journal Title
Glastechnische Berichte 1983 56K (1) 130-135
Sector
Primary Papers
Class
PP 569

Request article (free for British Glass members)

Influence Of Tank Geometry And The Electrode Arrangement On The Flow And Temperature Distribution At Different Loads In A Glass Tank Furnace
Glastechnische Berichte 1983 56K (1) 130-135
PP 569