Influence Of Redox Equilibirum On The Proeprties Of Glasses With A High Iron Concentration

In glasses of the system Na2O-CaO-SiO2-Fe2O3, Fe2+ & Fe3+ ions were found by Mossbauer spectroscopy. In samples melted in oxidising atmosphere, both ions occurred in tetrahedral coordination, whereas they occurred in coordination no. 6 in samples with high iron content & meted under reducing conditions. It is shown that a total iron concentration has a stronger influence on the glass properties than the redox state. Differences in the properties of glasses melted in oxidising & reducing atmosphere, were observed at lower temperatures, while at higher temperatures they are very small. Density, microhardness, transition temperature & thermal expansion coefficient of the glasses studied are affected by the changes in redox equilibrium. One can conclude that after reducing treatment iron ions present in the glass structure play a similar role as a network modifier.

Author
A Zawada Et Al
Origin
Tu-Bergakademie Freilberg, Germany
Journal Title
Glass Sci Technol 78 3 2005 106
Sector
Special Glass
Class
S 2972

Request article (free for British Glass members)

Influence Of Redox Equilibirum On The Proeprties Of Glasses With A High Iron Concentration
Glass Sci Technol 78 3 2005 106
S 2972
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 14 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.