Influence Of Process Parameters On The Formation Of Protective Mosix Layers On Molybdenum Electrodes During Electric Melting Of Glass Auteur(S) / Author(S)

With the aid of laboratory experiments, the cathodic passivation of molybdenum electrodes during electrical melting of glass was studied. The formation of molybdenum silicide layers does not only depend on the cathodic passivation currents, but also on time and the AC heating current density. If the melt has freshly been prepared from raw materials, the molybdenum silicide layer is thinner than under otherwise same conditions. While at an AC heating current density of 1 A/cm2, a cathodic current density of 3.75 mA/cm2 led to optimum layer formation. at a heating current density of 2 A/cm2, higher cathodic current densities are required.

Author
Un-named
Origin
C Rüssel & A Kämpfer
Journal Title
Glass Science & Technol 71 2 1998 35-41
Sector
General
Class
G 4163

Request article (free for British Glass members)

Influence Of Process Parameters On The Formation Of Protective Mosix Layers On Molybdenum Electrodes During Electric Melting Of Glass Auteur(S) / Author(S)
Glass Science & Technol 71 2 1998 35-41
G 4163
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.