Influence Of Phosphorus, Barium, And Lead Compositional Variation On The Chemical Durability Of A Multicomponent Glass System

Glasses were prepared by systematic additions of P205, Ba0, and Pb0 to glasses consisting of Al203-B203-(Ba0)-Ca0-Fe203-K20-Mg0-Na20-(Pb0)-P205)-Si02, and their chemical durability was examined by the EPA TCLP test. The addition of about 1 mol% P205 to a glass containing 5 mol% Pb0 increases the normalized lead leaching rate (NLLR) by about 40 relative%, but increasing P205 to 2 mol% decreases the NLLR to about the NLLR obtained without P205. A similar, but more dramatic behaviour with changes in the NLLR of about 300 relative% is obtained by sequential combined additions of 1 mol% each of P205 and BaO to a glass containing 1 mol% PbO.

Author
W Luo Et Al
Origin
Vitreous State Laboratory, Washington Dc
Journal Title
J Am Ceram Soc 1997 2148-2152
Sector
General
Class
G 1703

Request article (free for British Glass members)

Influence Of Phosphorus, Barium, And Lead Compositional Variation On The Chemical Durability Of A Multicomponent Glass System
J Am Ceram Soc 1997 2148-2152
G 1703
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.