Influence Of Montmorillonite Clay On Structure & Properties Of Sodium Borate Glasses

In the light of environmental perspective, clay minerals attract special interest because of their capability to absorb and chemically stabilize heavy metals in their structure. The absolute suppression of heavy element leakage from clay structures to the environment, which is obviously a strict demand, can be achieved with clay vitrification. This work is related to the influence of the addition of 0-50 st% of montmorillonite to a borate glass with composition of 0.33Na2O-0.67B2O3 on its structure.

Author
E Diamanti Et Al
Origin
University Of Ioannina, Greece
Journal Title
9Th Esg Conference, Trencin, Slovak Republic, June 2008 57-60
Sector
Special Glass
Class
S 3374

Request article (free for British Glass members)

Influence Of Montmorillonite Clay On Structure & Properties Of Sodium Borate Glasses
9Th Esg Conference, Trencin, Slovak Republic, June 2008 57-60
S 3374
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.