Influence Of Mixed Alkali Oxides On Some Melt Properties Of Tv Screen Glass

The influence of K20/R20(R20=Na20+K20) on some melt properties was studied in alkali-alkaline earth-silicate TV screen glasses. Viscosity, surface tension, electrical resisitivity, volatilization and devitrification of glass melts was determined.

Author
J H Hwant Et Al
Origin
Dept Ceramic Eng, Yonsei University, Korea
Journal Title
Glastech Ber Glass Sci Technol 73 1 2000 8-17
Sector
Special Glass
Class
S 1894

Request article (free for British Glass members)

Influence Of Mixed Alkali Oxides On Some Melt Properties Of Tv Screen Glass
Glastech Ber Glass Sci Technol 73 1 2000 8-17
S 1894