Influence Of Internal Strucutre On Flaw Information In Commercial Glasses

Some commercial plate-glass possess a structure which appears to influence the shape and directional characteristics of minute flaw formations. Geometrically oriented flaws which are believed to be due to micro inhomogeneities in the structure were found around localised stress regions. The influence of these inhomogeneous regions is reduced, but not completely removed, by remelting the glass. A dynamic spherical indentor technique was used to produce flaws under controlled conditions on various commercial glasses. The product of average flaw length and flaw number was taken as a relative measure of the total bonds broken with the given stress conditions. In remelted glasses, a linear relationship was obtained between the logarithm of flaw length and the reciprocal of melting-temperature.

Author
W.C. Levengood And T.S. Vong
Origin
Unknown
Journal Title
Physics And Chem Glasses, 1, 189, 1960)
Sector
Primary Papers
Class
PP 332

Request article (free for British Glass members)

Influence Of Internal Strucutre On Flaw Information In Commercial Glasses
Physics And Chem Glasses, 1, 189, 1960)
PP 332
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.