Influence Of Glass Frits On Working Properties Of Kaolins

This paper presents a report of the effects of glass frits on the properties of some Nigerian clays. Eight test pieces of various compositions with 10, 20, 30, up to 80% glass frit addition were prepared and analyzed. The samples were tested for properties such as cold crushing strength, linear shrinkage, fusion point and loss on ignition. The samples with 50% glass frits showed optimum strength and lowest shrinkage. The minimum strength was obtained from the sample with 80% glass frit. The optimal operating temperature for all the samples was 1000 °C. Thus Nigerian clays reinforced with appropriate quantities of glass frits are suitable for different low temperature applications such as in electrical heating devices, vitrified tiles and tablewares.

Author
Un-named
Origin
Unknown
Journal Title
Applied Clay Science 52, (4) June 2011 428-431
Sector
Domestic glass
Class
D 1238

Request article (free for British Glass members)

Influence Of Glass Frits On Working Properties Of Kaolins
Applied Clay Science 52, (4) June 2011 428-431
D 1238
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.