Influence Of The Eu2+ On The Silver Aggregates Formation In Ag+-Na+ Ion-Exchanged Eu3+-Doped Sodium-Aluminosilicate Glasses

Europium-doping sodium-aluminosilicate glasses are parepared by melt-quenching method, in which europium ions were spontaneously reduces from their trivalent to divalent state. Interactions between europium ions and silver species were investigated.

Author
L Li Et Al
Origin
Kunming University Science & Technology, Kunming, China
Journal Title
J Am Ceram Soc 97 4 2014 1110-1114