Influence Of Cullet On The Glass Melting Process

This article looks at the low-temperature reactions taking place in the mixture of raw materials (batch and cullet) after their inlet into the glass melting furnace. It has been assumed that, in the first melting stage, there are some batch components that react earlier and at lower temperatures with the cullet. The retarding effect of the silicates formed in this advanced stage on the kinetics of the sand dissolution is compensated by the influence on the intensification measures, i.e by increasing melting temperatures in general.

Author
S Gelnar & E Smrckova
Origin
Arcadia Co & Fchpt, Slovakia
Journal Title
Glass International March 2010 15-16, 18-20
Sector
Container glass
Class
C 4111

Request article (free for British Glass members)

Influence Of Cullet On The Glass Melting Process
Glass International March 2010 15-16, 18-20
C 4111
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.