Influence Of Copper On The Redox Buffering By Sulphate And Carbonate Of Reduced Soda-Lime-Silica Glasses

A study has been made of the effect of sulphate and carbonate on the redox properties of glasses, with the molybdenum used by the authors in their previous work replaced by copper.