Influence Of Cooling Rate On The Thermodynamic Properties Of Silver Metaphosphate Glass

Silver metaphosphate is a well known model system for studying the thermodynamic properties of phosphate glasses which are of interest for applications as solid electolytes. In particular, the glass transition temperature (Tg), the heat capacity (Cp) and the limiting fictive temperature (Tf) display a dependence upon the details of preparation. Differential scanning calorimetry was used to determine the effects of cooling rate on some thermodynamic properties of the resulting glass.

Author
C Tomasi Et Al
Origin
Cste-Cnr, Italy
Journal Title
Phys Chem Glasses 36 3 1995 136-138
Sector
Special Glass
Class
S 873

Request article (free for British Glass members)

Influence Of Cooling Rate On The Thermodynamic Properties Of Silver Metaphosphate Glass
Phys Chem Glasses 36 3 1995 136-138
S 873
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.