Influence Of Cations On The Optical Properties Of Nd3+, Eu3+ And Er3+ Doped Borate Glasses

Nd3+ absorption maxima in Li20-b203, CaO-B203 and Ba0-B203 glasses show a red shift with increasing cationic size.